Description: This DSC measures glass transition temperature, melting temperature, peak areas, crystallinaty, and specific heat capacities of various substances. The temperature range is from -170C to 700C. Gas purge options include N2, Ar, He, or Air with optional LN2 cooling. The machine is able to use 30 and 100 microliters crucibles with high pressure resistance up to 7250psi.
POC: Jeff Hinkley
E-mail: jeffrey.a.hinkley@nasa.gov
Location: Bldg 1293C; Rm 270
Training: Training Required
Manufacturer: Setaram
Model: DSC 131 |
 |
|